NORYL
| PHYSICAL | |
| SPECIFIC GRAVITY | 1.05 - 1.10 |
| WATER ABSORPTION, 24 hr. (%) | 0.07 |
| MECHANICAL | |
| TENSILE | |
| Strength, Yield (10³ psi) @ 73°F. | 6.5 - 9.6 |
| Elongation, Ultimate (%) @ 73°F. | |
| Modulus, Yield (10³ psi) @ 73°F. | |
| FLEXURAL | |
| Strength, (10³ psi) @ 73°F. | 8.3 - 13.5 |
| Modulus, Yield (10³ psi) @ 73°F. | 340 - 360 |
| COMPRESSIVE STRENGTH — 2% Offset (10³ psi) | |
| IMPACT STRENGTH — Izod, Notched (ft.-lb./in.) @ 73°F. | 5.0 - 7.0 |
| HARDNESS | R113/119 |
| COEFFICIENT OF STATIC FRICTION — Against self | |
| Against steel | |
| THERMAL | |
| CONDUCTIVITY (BTU/hr/sq. ft./Degree F./in.) | |
| COEFF. OF THERMAL EXPANSION (10⁻⁵/Degree F.) | 3.3 - 4.1 |
| SPECIFIC HEAT (BTU/lb./Degree F.) | |
| HEAT DEFLECTION TEMP. (Degree F.) | |
| At 66 psi. | 200 - 279 |
| At 264 psi | 185 - 265 |
| MAX. CONTINUOUS TEMP. (F.°) | 122 - 221 |
| ELECTRICAL | |
| VOLUME RESISTIVITY (Ohm/cm) | |
| DIELECTRIC STRENGTH (V/Mil) | 400 - 630 |
| DIELECTRIC CONSTANT — At 60 HZ | 2.65 - 2.8 |
| DIELECTRIC CONSTANT — At 1 MHZ | 3.7 - 3.9 |
| DISSIPATION FACTOR — At 60 HZ | .0004 - .0007 |
| DISSIPATION FACTOR — At 1 MHZ | .0024 |
| ARC RESISTANCE (seconds) | |